Fixing warping and moisture problems
Many nylon printing problems come from moisture or uneven cooling. Work through these checks in order.
Corners lifting off the bed
- Clean the bed according to the bed maker's instructions.
- Check the first layer. It should be lightly pressed down, not round and loose. Re-level or adjust Z offset if needed.
- Use a suitable surface such as garolite, or PEI with glue stick or a nylon-specific adhesive.
- Add a brim or corner "mouse ears."
- Raise the bed temperature slightly while staying within the limits recommended by your printer and filament manufacturer.
- Close the enclosure and preheat it before printing.
Layers splitting or cracking
- Stop drafts by closing the enclosure and keeping the printer away from fans and vents.
- Reduce part cooling.
- Raise the nozzle temperature in small steps within the maker's recommended range.
- Dry the filament. Moisture can weaken layer bonding.
Bubbles, popping, or rough surfaces
These are common signs that the filament has absorbed moisture. Dry the spool following the maker's guidance, then print from a sealed dry box. See drying and storing nylon.
Stringing
- Dry the filament first; moisture often makes stringing worse.
- Lower the nozzle temperature slightly within the recommended range.
- Tune retraction in small steps, within your extruder maker's recommendations.
Under-extrusion or clogs with CF-nylon
- Check the nozzle for wear; fiber-filled nylon can wear brass nozzles. A hardened nozzle is strongly recommended.
- Some makers recommend a larger nozzle diameter, such as 0.6 mm, for fiber-filled filament. Check your filament maker's guidance.
Design changes that help
- Round sharp outside corners with fillets.
- Avoid very long, flat, thin shapes, or split them into parts.
- Orient the part so its largest flat face sits on the bed.
Back to the nylon printing guide.